Add to Cart
Alloy C276 Hastelloy C Pipe B574 / B575 / B619 / B622 , High
Performance
High Performance Alloys stocks and produces this grade in the
following forms: Bar, wire, sheet, plate, coil,
fasteners and forgings. Request quote on this grade. See our
on-line catalog for sizes stocked.
Overview
Nickel-chromium-molybdenum wrought alloy that is considered the
most versatile corrosion resistant alloy available. This alloy is
resistant to the formation of grain boundary precipitates in the
weld heat-affected zone, thus
making it suitable for most chemical process applications in an as
welded condition. Alloy C-276 also has excellent resistance to
pitting, stress corrosion cracking and oxidizing atmospheres up to
1900F. Alloy C-276 has exceptional resistance to a
wide variety of chemical environments.
Characteristics
Applications
Some typical applications include equipment components in chemical
and petrochemical organic chloride
processes and processes utilizing halide or acid catalysts. Other
industry applications are pulp and paper
(digesters and bleach areas), scrubbers and ducting for flue gas
desulfurization, pharmaceutical and food
processing equipment.
HASTELLOY Alloy C-276 is a nickel-chromium-molybdenum alloy with
universal corrosion resistance unmatched by any other alloy. It has
outstanding
resistance to a wide variety of chemical process environments
including ferric and cupric chlorides, hot
contaminated mineral acids, solvents, chlorine and chlorine
contaminated (both organic and inorganic),
dry chlorine, formic and acetic acids, acetic anhydride, sea water
and brine solutions and hypochlorite and
chlorine dioxide solutions. Alloy C-276 also resists formation of
grain boundary precipitates in the weld
heat affected zone making it useful for most chemical processes in
the as-welded condition. It has
excellent resistance to pitting and stress corrosion cracking.
HASTELLOY Alloy C-276 sheet 0.044" thick in the heat-treated
condition at 2050 F, rapid quenched, has
an average olsen cup depth of 0.48". C-276 can be successfully
fabricated by many methods. The alloy
tends to work harden but with the proper care, the alloy is readily
hot and cold formed. Complete
information on welding, machining and forming is available
Chemistry
Chemical Requirements | |||||||
Ni | Cr | Mn | Mo | C | Si | Fe | |
Max | Bal. | 16.5 | 1.0 | 17.0 | 0.010 | 0.08 | 7.0 |
Min | 14.5 | 15.0 | 4.0 |
Tensile Data
Mechanical Property Requirements | |||||
Ultimate Tensile | Yield Strength (0.2% OS) | Elong. in 2 in. (50.8mm) or 4D min,% | R/A | Hardness | |
Min | 100 KSi | 41 KSi | 40 | ||
Max | |||||
Min | 690 MPa | 283 MPa | |||
Max |
Specifications
Form | Standard |
Metal Type | UNS N10276 |
Bar | ASTM B574 Din 17752 |
Wire | |
Sheet | ASTM B575 Din 17750 |
Plate | ASTM B575 Din 17750 |
Fitting | ASTM B366 |
Forging | ASTM B564 |
Tube | ASTM B619 ASTM B622 ASTM B626 Din 17751 |
Pipe | ASTM B619 ASTM B622 ASTM B626 Din 17751 |
Weld Wire | A5.14 ERNiCrMo-4 |
Weld Electrode | A5.11 ENiCrMo-4 |
Din. | 2.4819 All Forms |