Chemical composition
Composition | C | P | S | Mn | Si |
≤ | |||||
Content(%) | 0.03 | 0.02 | 0.02 | 0.3~0.6 | 0.15~0.3 |
composition | Ni | Cr | Mo | Cu | Fe |
Content(%) | 79.0~81.0 | - | 4.8~5.2 | ≤0.2 | Bal |
shop sign | Annealing medium | heating temperature | Keep the temperature time/h | Cooling rate |
1j85 | Dry hydrogen or vacuum, pressure is not greater than 0.1 Pa | Along with the furnace heating up 1100~1150ºC | 3~6 | In 100 ~ 200 ºC / h speed cooling to 600 ºC, fast to 300 ºC draw a charge |
Style of supply
Alloys Name | Type | Dimension | ||
1J85 | Wire | D= 0.1~8mm | ||
1J85 | Strip | W= 8~390mm | T= 0.3mm | |
1J85 | Foil | W= 10~100mm | T= 0.01~0.1 | |
1J85 | Bar | Dia= 8~100mm | L= 50~1000 |
Soft magnetic alloy outer magnetic field under the action of easy
magnetization, basic disappear after removal of magnetic field of
magnetic induction intensity and magnetic alloys.
Application: Pulse transformer, Relays, Transformers, Magnetic amplifier, Electromagnetic clutch, Choke core and magnetic shielding, Automotive sensors.