Welding wire Aws 5.14 Nickel Alloy Wire Ernicrmo-4 for Nickel Base Alloys
INTRODUCTION
ERNiCrMo-4 is used for gas-tungsten-arc and gas-metal-arc welding
of Inconel alloy C-276 and other nickel-chromium-molybdenum alloys.
Due to high molybdenum content, this alloy offers excellent
resistance to stress corrosion cracking and pitting and crevice
corrosion.
Common Names: Oxford Alloy® C-276 FM C-276 Techalloy 276
Standard: AWS A5.14, ERNiCrMo-4/ ASME II, SFA-5.14, UNS N10276
Werkstoff Nr. 2.4886 ISO SNi6276 Europe NiCrMo16Fe6W4
CHEMICAL COMPOSITION(%)
C | Si | Mn | S | P | Ni | Co |
≤0.02 | ≤0.08 | ≤1.0 | ≤0.03 | ≤0.04 | Rest | ≤2.5 |
W | V | Fe | Cu | Cr | Mo | others |
3.0-4.5 | ≤0.35 | 4.0-7.0 | ≤0.5 | 14.5-16.5 | 15-17 | <0.5 |
WELDING PARAMETERS
Process | Diameter | Voltage | Amperage | Gas |
TIG | .035" (0.9mm) .045" (1.2mm) 1/16" (1.6mm) 3/32" (2.4mm) 1/8" (3.2mm) | 12-15 13-16 14-18 15-20 15-20 | 60-90 80-110 90-130 120-175 150-220 | 100% Argon 100% Argon 100% Argon 100% Argon 100% Argon |
MIG | .035" (0.9mm) .045" (1.2mm) 1/16" (1.6mm) | 26-29 28-32 29-33 | 150-190 180-220 200-250 | 75% Argon + 25% Helium 75% Argon + 25% Helium 75% Argon + 25% Helium |
SAW | 3/32" (2.4mm) 1/8" (3.2mm) 5/32" (4.0mm) | 28-30 29-32 30-33 | 275-350 350-450 400-550 | Suitable Flux may be used Suitable Flux may be used Suitable Flux may be used |
MECHANICAL PROPERTIES
Tensile Strength | 114,500 PSI | 790 MPA |
Yield Strength | 85,000 PSI | 590 MPA |
Elongation | 27% |
APPLICATIONS
ERNiCrMo-4 of its high molybdenum content it offers excellent
resistance to stress corrosion cracking, pitting, and crevice
corrosion, thus it is often used for cladding.
ERNiCrMo-4 offen used for groove welding of 9% nickel steels in the
production of LGN storage tanks.
ERNiCrMo-4 also can be used for welding of materials of similar
chemical composition, as well as dissimilar material of nickel base
alloys, steels and stainless steels.