965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance

Brand Name:BLM-DX-1
Minimum Order Quantity:100kgs
Delivery Time:25-30 days subject to the clients' requirement and quantity
Payment Terms:Western Union, L/C, T/T
Place of Origin:Jiangsu, China (Mainland)
Price:FobShanghai usd 5.9-6.4/kg
Contact Now

Add to Cart

Verified Supplier
Address: B615, Future Fortune Building, No. 1 Wangxi Road, Zhangjiagang City, Jiangsu Province
Supplier`s last login times: within 27 hours
Product Details Company Profile
Product Details

Inconel 718

Inconel 718 Chemical composition


Alloy%NiCrFeMoNbCoCMnSiSCuAlTi
718Min.5017balance2.84.750.20.7
Max.55213.35.510.080.350.350.010.30.81.15

Inconel 718 Physical properties


Density8.2 g/cm³
Melting point1260-1340 ℃

Inconel 718 Alloy minimum mechanical properties in the roomtemperature


AlloyTensile strength Rm N/mm²Yield strength R P0. 2N/mm²Elongation A 5 %

Brinell hardness

HB

Solution treatment96555030≤363

718 Characteristic as below:

1.workability

2.High tensile strength,endurance strength,creep strength and rupture strength at 700℃.

3.High inoxidability at1000℃. 4.Steady mechanical performance in the low temperature.

5.Good welding performance.


Inconel 718 Metallurgical structure


718alloy is Austenitic structure, precipitation hardening generate "γ" made it excellent mechanical performance. G rain boundary generate "δ" made it the best plasticity in the heat treatment.


Inconel 718 Corrosion resistance


718 alloy with extremely resistance to stress corrosion cracking and pitting ability in high temperature or low temperature environments, especially the inoxidability in the high temperature.


Inconel 718 Application field:

1 . The elevated temperature strength, excellent corrosion resistance and workability at 700℃ properties

2 . made it use in a wide range of high requirement environments :Steam turbine ; Liquid-fuel rocket ; Cryogenic engineering

3.Acid environment

4.Nuclear engineering



China 965 Tensile Strength Inconel Nickel Alloy Inconel 718 Tube With Stress Corrosion Cracking Resistance supplier