Add to Cart
Ⅰ Product description
is the key equipment of wood anticorrosion and coloring. Through the pharmaceutical infusion, pressure infiltration, vacuum
drying and other processes, the wood in the storage tank can not only effectively prevent the
mildew corrosion caused by wood rot bacteria, but also effectively
prevent the damage of termites, wood borers and other insects to
the wood. At the same time, adding different agentia can have the
effect of flame retardant and coloring, greatly improving the
service life and use effect of wood. Anticorrosive and flame retardant wood is widely used in indoor furniture, wood,
antique garden construction, railways, mines, dock protection wood,
pile of timber construction and other occasions.
Ⅱ Main Model
Model | Total capacity (m3) | Treat capacity(m3) |
DN 1200*6000mm | 6.7 | 4.5 |
DN 1200*8000mm | 9.0 | 6.0 |
DN 1500*4000mm | 7.0 | 4.71 |
DN 1500*6000mm | 10.5 | 7.0 |
DN 1500*8000mm | 14 | 9.4 |
DN 1800*4000mm | 10.1 | 6.78 |
DN 1800*6000mm | 15.2 | 10.17 |
DN 1800*8000mm | 20.3 | 13.5 |
DN 2000*6000mm | 18.8 | 12.5 |
DN 2000*8000mm | 25 | 16.7 |
DN 2000*10000mm | 31.4 | 20 |
DN 2000*18000mm | 56 | 37 |
Note: The diameter and length can be customized according to users'
needs. If the above model is not suitable, please tell us the
diameter and length you need. We can customize it for you.
Ⅲ Technical parameters
Ⅳ
Technology Process
Wood cooking equipment
The reason why the wood should be cooked is mainly because the
color of the wood can be changed after cooking; the color
difference between the core and sapwood of the wood can be reduced;
the luster of the wood can be maintained; the gradient difference
of the initial moisture content of the wood can be alleviated; the
probability of the occurrence of wood drying defects can be
reduced; at the same time, it is not easy to crack after cooking,
which also helps to prevent corrosion and moth.
The purpose of cooking is to soften the wood, increase the
plasticity and moisture content of the wood, reduce the cutting
resistance during planing, and remove the oil, tannin and other
extracts from a part of the wood.
1. Change the color of wood (purely physical method).
2. The color difference of wood core and sapwood was reduced.
3. Keep the natural luster of wood.
4. It can alleviate the gradient difference of initial moisture
content of wood.
5. Reduce the probability of wood drying defects.
6. Shorten wood drying cycle