317L Stainless Steel Heat Exchanger Tube With Stress Corrosion Resistance For Chemical

Brand Name:Zheheng
Certification:ISO9001
Model Number:317L
Minimum Order Quantity:MOQ500kg
Delivery Time:7-15 working days after receiving payment
Payment Terms:L/C, D/P, T/T, Western Union
Contact Now

Add to Cart

Verified Supplier
Location: Wenzhou Zhejiang China
Address: No999 .wenzhou airport wenzhou city,zhejiang china
Supplier`s last login times: within 25 hours
Product Details Company Profile
Product Details

317L Stainless steel pipe Characteristic


Stainless steel grade 317L is a low carbon version of grade 317 stainless steel.It can produce stronger welds due to the low carbon content. It has higher ductility, stress corrosion resistance, compressive strength and high temperature resistance


Grade S31703 stainless steel is widely used in the following applications


1) Oil and gas industry equipment;
2) Offshore platforms, heat exchangers, underwater equipment, firefighting equipment;
3) Chemical processing industry, utensils and pipeline industry;
4) Desalting, high pressure RO equipment and submarine pipelines;
5) Energy industry such as power plant desulfurization and denitration FGD system, industrial scrubbing system, absorption tower;
6) Mechanical parts that require high strength, corrosion resistant and anti-wear performance;

317L stainless pipe Chemical Composition


N0.10
C0.03
Mn2
P0.045
S0.03
Si0.75
Cr18.0-20.0
Ni11-15
Mo3.0-4.0



Mechanical Properties Stainless steel 317L


MaterialUltimate Tensile Strength(Mpa)0.2%Yield Strength (Mpa)%Elongation in2''Rockwell B Hardness
Alloy 317L5152054095


Product Testing


Hydrostatic test
Flaw detection test
Lab test

Package Process


1.with plastic cap to protect both ends

2.weaving bag wrapped outside the pipe

3.then pack into wooden case.


Image


China 317L Stainless Steel Heat Exchanger Tube With Stress Corrosion Resistance For Chemical supplier

317L Stainless Steel Heat Exchanger Tube With Stress Corrosion Resistance For Chemical

Inquiry Cart 0