AOMT123608 Tungsten Carbide Inserts Filling Customize For Cnc Cutter Tool

Brand Name:BWIN
Model Number:AOMT123608
Minimum Order Quantity:10pcs/box
Delivery Time:7 work days
Payment Terms:T/T, Western Union
Place of Origin:China
Contact Now

Add to Cart

Verified Supplier
Location: Shenzhen China
Address: No.1613, honghai Bldg., Songgang Rd., Baoan Area, Shenzhen , China
Supplier`s last login times: within 1 hours
Product Details Company Profile
Product Details

Quick Detail:

Good process performance

Strong universality

High processing finish

High stability

High-precision

High efficiency


Description:

It is made of high-quality tungsten steel alloy, which is wear-resistant and durable overall, with smooth and polished surface and effective corrosion resistance; New coating and new substrate technology, high hardness, wear resistance, more stable processing; Smooth chip removal, stable cutting, good chip breaking effect, and rapid improvement of processing efficiency.


Specifications:​

BrandBWIN
ModelAOMT123608
ColorBrown/Fuchsia
WorkpieceSteel/Stainless steel
TypeMilling Insert
MaterialTungsten Carbide Milling Insert
ProcessingMedium Cutting
FeatureHigh Hardness
Good Toughness
Good process performance

High efficiency

Shock and vibration resistance
StandardISO
Quantity10pcs/box
Weight0.015kg
PackagePlastic Box
CustomizedOEM, ODM

Notice:

1. The carbide milling inserts shall not be collided or dropped on the ground and must be handled with care.

2. Before installing the carbide milling inserts, the performance and purpose of the saw table must be confirmed to ensure that the cutting direction indicated by the blade arrow is consistent with the rotation direction of the saw table. It is strictly prohibited to install in the opposite direction. Wrong installation direction may cause the blade sawtooth to fall off, so as to prevent accidents.

3. After installation, it is necessary to confirm whether the central hole of the carbide milling inserts is firmly fixed on the flange plate of the saw table. If there is a gasket, the gasket must be sleeved; Then, gently push with your hand to confirm whether the blade rotates eccentrically.

4. When using, do not exceed the specified high speed

5. When the carbide milling inserts is not used, hang the blade vertically on the dry shelf.


Applications:

Our carbide milling inserts could to be processed Alloy steel, Tool steel, carbon steel, stainless steel, Cast iron and Titanium alloy. Working material as following:


FAQ
1. Flank Wear? Higher cutting resistance,Notch wear on flank,Poor roughness of surface, or deterioration of accuracy.
Soft grades,Excessive cutting speed,Small flank angle,Low feed.
Select a higher,wear-resistant grade,Reduce cutting speed,Increase flank angle,Increase feed.
2. Crater Wear? Uncontrolled chip,Poor surface quality,when finishing High speed processing carbon steel
Soft grades,Excessive cutting speed,Excessive feed,The strength of chip breaker Insufficiet.
Change to a higher wear-resistant grade,Reduce cutting speed,Reduce feed,Select a higher strength chip breaker.
3. Chipping? Sudden fracture of cutting edge(rake face and flank),Instability insert life
Toughness insufficient,Excessive feed rate,Strength of cutting edge insufficient,Instability of the tool.
Select a tougher grade,Decrease feed rate,Increase honing of cutting edge(chamfering to rounding),Increase the stability and setting angle
4. Insert Fracture? Cutting resistance increased Poor surface roughness.
Toughness insufficient,Excessive feed rate,Strength of cutting edge insufficient,Instability of the tool.
Select a tougher grade,Decrease feed rate,Increase honing of cutting edge(chamfering to rounding),Increase the stability and setting angle.
5. Plastic Deformation? Variation of dimension Nose wear,cutting edge drape or passivating.when processing alloy steel Poor surface roughness
Soft grade,Excessive cutting speed,Excessive cutting depth and feed rate,Overheat on cutting edge.
Select a higher red hardness cutting material,Decrease cutting speed,Decrease cutting depth and feed rate,Select a higher thermal conductivity cutting material(CVD+sufficient coolant).
6. Build-Up-Edge? Workpiece dissove with Cutting edge Poor surface roughness when finishing,Cutting resistance increased,Cutting soft materials.
Cutting speed too low,Cutting edge obtuse,Unsuitable tool material. Increase cutting speed,Increase rake angle,Select small sticking force.