Blmp0603 Carbide Milling Insert Cnc Blmp0904 High Efficiency

Brand Name:BWIN
Model Number:BLMP0904
Minimum Order Quantity:10pcs/box
Delivery Time:7 work days
Payment Terms:T/T, Western Union
Place of Origin:China
Contact Now

Add to Cart

Verified Supplier
Location: Shenzhen China
Address: No.1613, honghai Bldg., Songgang Rd., Baoan Area, Shenzhen , China
Supplier`s last login times: within 1 hours
Product Details Company Profile
Product Details

Tungsten Carbide Milling Insert Blmp0603 Blmp0904 Cnc Cutting Tools High Efficiency


Quick Detail:

  • High hardness tool body
  • Not easy to deform
  • Power milling
  • Smooth chip breaking
  • High speed machining

Description:

  • The carbide lathe insert is finely ground by imported technology, with stronger overall hardness, higher stiffness and better toughness; The coating is thicker and more stable when the stress below 1000 ° is deposited and sprayed back to the temple; Double sided four edge machining is more economical and practical, with small cutting resistance and high efficiency; High precision blade can effectively reduce friction, reduce blade loss, and extend the service life of the blade.

Specifications:​

BrandBWIN
ModelBLMP0603R BLMP0903R
ColorYellow/Black
WorkpieceSteel/Cast Iron
TypeMilling Insert
MaterialMilling Tungsten Carbide Lathe Insert
ProcessingMedium Cutting
FeatureHigh hardness tool body
Not easy to deform
Power milling

Smooth chip breaking

High speed machining
StandardISO
Quantity10pcs/box
Weight0.015kg
PackagePlastic Box
CustomizedOEM, ODM

Lead Time:

antity(pieces)1 - 3000>3000
Lead time (days)7To be negotiated

Notice:

  • The milling tungsten carbide lathe insert shall not be collided or dropped on the ground and must be handled with care.
  • Before installing the milling tungsten carbide lathe insert , the performance and purpose of the saw table must be confirmed to ensure that the cutting direction indicated by the blade arrow is consistent with the rotation direction of the saw table. It is strictly prohibited to install in the opposite direction. Wrong installation direction may cause the blade sawtooth to fall off, so as to prevent accidents.
  • After installation, it is necessary to confirm whether the central hole of the carbide lathe insert is firmly fixed on the flange plate of the saw table. If there is a gasket, the gasket must be sleeved; Then, gently push with your hand to confirm whether the blade rotates eccentrically.
  • When using, do not exceed the specified high speed
  • When the milling tungsten carbide lathe insert is not used, hang the blade vertically on the dry shelf.

Applications:

Our milling tungsten carbide lathe insert could to be processed Alloy steel, Tool steel, carbon steel, stainless steel, Cast iron and Titanium alloy. Working material as following:


FAQ
1. Flank Wear? Higher cutting resistance,Notch wear on flank,Poor roughness of surface, or deterioration of accuracy.
Soft grades,Excessive cutting speed,Small flank angle,Low feed.
Select a higher,wear-resistant grade,Reduce cutting speed,Increase flank angle,Increase feed.
2. Crater Wear? Uncontrolled chip,Poor surface quality,when finishing High speed processing carbon steel
Soft grades,Excessive cutting speed,Excessive feed,The strength of chip breaker Insufficiet.
Change to a higher wear-resistant grade,Reduce cutting speed,Reduce feed,Select a higher strength chip breaker.
3. Chipping? Sudden fracture of cutting edge(rake face and flank),Instability insert life
Toughness insufficient,Excessive feed rate,Strength of cutting edge insufficient,Instability of the tool.
Select a tougher grade,Decrease feed rate,Increase honing of cutting edge(chamfering to rounding),Increase the stability and setting angle
4. Insert Fracture? Cutting resistance increased Poor surface roughness.
Toughness insufficient,Excessive feed rate,Strength of cutting edge insufficient,Instability of the tool.
Select a tougher grade,Decrease feed rate,Increase honing of cutting edge(chamfering to rounding),Increase the stability and setting angle.
5. Plastic Deformation? Variation of dimension Nose wear,cutting edge drape or passivating.when processing alloy steel Poor surface roughness
Soft grade,Excessive cutting speed,Excessive cutting depth and feed rate,Overheat on cutting edge.
Select a higher red hardness cutting material,Decrease cutting speed,Decrease cutting depth and feed rate,Select a higher thermal conductivity cutting material(CVD+sufficient coolant).
6. Build-Up-Edge? Workpiece dissove with Cutting edge Poor surface roughness when finishing,Cutting resistance increased,Cutting soft materials.
Cutting speed too low,Cutting edge obtuse,Unsuitable tool material. Increase cutting speed,Increase rake angle,Select small sticking force.

China Blmp0603 Carbide Milling Insert Cnc Blmp0904 High Efficiency supplier

Blmp0603 Carbide Milling Insert Cnc Blmp0904 High Efficiency

Inquiry Cart 0