Add to Cart
Quick Detail
Description
Specifications:
Brand | BWIN |
Model | WNMG080408 |
Color | colorful |
Workpiece | Cast iron/Steel/Stainless steel/Aluminium |
Type | Cnc Carbide Turning Cutting Tool |
Material | Tungsten Carbide Insert |
Processing Type | Medium Cutting |
Feature | Good red hardness |
High strength blade | |
Anti collapse and wear resistance | |
Smooth cutting | |
Durable and wear-resistant | |
Standard | ISO |
Quantity | 10pcs/box |
Weight | 0.015kg |
Package | Plastic Box |
Customized Support | OEM, ODM |
Lead Time
antity(pieces) | 1 - 3000 | >3000 |
Lead time (days) | 7 | To be negotiated |
Parameters
WN□□0804◯◯ | |||
I(mm) | s(mm) | ic(mm) | d1(mm) |
8.7 | 4.76 | 12.7 | 5.16 |
WN□□0604◯◯ | |||
I(mm) | s(mm) | ic(mm) | d1(mm) |
6.5 | 4.76 | 9.525 | 3.81 |
Notice
Be careful not to mix two or several tungsten carbide inserts together
Pay special attention to the protection of the cutting edge; Never touch or fall on the ground
The service life of milling cutter can be prolonged by appropriately reducing the cutting speed and feed speed
The cutting fluid shall be added to protect the tungsten carbide inserts edge during operation, so that the cutting is more smooth
When oxide film or other hardening layer remains on the workpiece surface, it shall be removed by reversible milling
Applications
Our tungsten carbide inserts could to be processed Alloy steel, Tool steel, carbon steel, stainless steel, Cast iron and Titanium alloy. Working material as following:
FAQ
1. Flank Wear?
Higher cutting resistance,Notch wear on flank,Poor roughness of surface, or deterioration of accuracy.
Soft grades,Excessive cutting speed,Small flank angle,Low feed.
Select a higher,wear-resistant grade,Reduce cutting speed,Increase flank angle,Increase feed.
2. Crater Wear?
Uncontrolled chip,Poor surface quality,when finishing High speed processing carbon steel
Soft grades,Excessive cutting speed,Excessive feed,The strength of chip breaker Insufficiet.
Change to a higher wear-resistant grade,Reduce cutting speed,Reduce feed,Select a higher strength chip breaker.
3.Insert Fracture?
Cutting resistance increased Poor surface roughness.
Toughness insufficient,Excessive feed rate,Strength of cutting edge insufficient,Instability of the tool.
Select a tougher grade,Decrease feed rate,Increase honing of cutting edge(chamfering to rounding),Increase the stability and setting angle.
4.Plastic Deformation?
Variation of dimension Nose wear,cutting edge drape or passivating.when processing alloy steel Poor surface roughness
Soft grade,Excessive cutting speed,Excessive cutting depth and feed rate,Overheat on cutting edge.
Select a higher red hardness cutting material,Decrease cutting speed,Decrease cutting depth and feed rate,Select a higher thermal conductivity cutting material(CVD+sufficient coolant).