Add to Cart
Customizable And High-Performance Long Fiber Geotextile For Filteration And Isolation
Product Introduction
Long fiber geotextile production line adopts the international advanced technology and domestic application of the double screw extrusion technology for the first time, double alignment system, pipeline air draft technology, plate wire pendulum system and high-speed needle into the cloth production process and so on 18 items international and domestic patent technology.
Product Properties
High strength, aging resistance, acid and alkali resistance, wear resistance, good flexibility, easy construction.
Product Application
Especially suitable for landfill, salt marsh, but also widely used in roads, railways, dams, tidal flats and other projects of filteration, isolation, and drainage and so on.
Product Specification
* Grams/㎡: 100g~800g/㎡
* Width: 1.0m~6.60m
* Roll length: 50m~200m (customized request accept)
PS: Customized request accept for all above.
Product Specification and Technical Index(GB/T 17639—2023)
Item | Index | ||||||||||
Nominal strength/(KN/m) | |||||||||||
6 | 9 | 12 | 18 | 24 | 30 | 36 | 48 | 54 | |||
1.00 | Longitudinal And Transverse Tensile Strength(KN/m≥) | 6.0 | 9.0 | 12.0 | 18.0 | 24.0 | 30.0 | 36.0 | 48.0 | 54.0 | |
2.00 | Elongation Under Maximum Load In Vertical And Horizontal Direction(%) | 30~80 | |||||||||
3.00 | CBR Burst Strength ( KN≥) | 0.9 | 1.6 | 1.9 | 2.9 | 3.9 | 5.3 | 6.4 | 7.9 | 8.5 | |
4.00 | Tearing Strength (KN,≥,LD/TD) | 0.15 | 0.22 | 0.29 | 0.43 | 0.57 | 0.71 | 0.83 | 1.10 | 1.25 | |
5.00 | Sieve SizeO90,O95 (mm) | 0.05~0.30 | |||||||||
6.00 | Vertical Permeability Coefficient (cm/s) | Kx(10ˉ1-10ˉ3) K=1.00-9.90 | |||||||||
7.00 | Width Variation (%≥) | -0.5 | |||||||||
8.00 | Weight Variation (%≥) | -5 | |||||||||
9.00 | Thickness Deviation Rate(%≥) | -10 | |||||||||
10.00 | Coefficient Of Thickness Variation(%≤) | 10 | |||||||||
11.00 | Dynamic Punch | Hole Diameter(mm≤) | 37.0 | 33.0 | 27.0 | 20.0 | 17.0 | 14.0 | 11.0 | 9.0 | 7.0 |
12.00 | Longitudinal And Transverse Breaking Strength(KN)≥ | 0.3 | 0.5 | 0.7 | 1.1 | 1.4 | 1.9 | 2.4 | 3.0 | 3.5 | |
13.00 | Uv resistance (Xenon Arc Lamp Method) | Vertical And Horizontal Strength Retention(%≥) | 70 | ||||||||
14.00 | Uv resistance (Fluorescent UV Lamp Method) | Vertical And Horizontal Strength Retention(%≥) | 80 |