Add to Cart
The Curie Temperature of SmCo Magnet ranges from 700-800°C, making it an ideal choice for high temperature applications. It can maintain its magnetic properties even at extreme temperatures, making it suitable for use in harsh environments.
SmCo Magnet can be magnetized in multipolar or so configurations, giving it a unique and flexible magnetization pattern. This allows for more precise control over the magnetic field and makes it suitable for a wide range of applications.
One of the key advantages of SmCo Magnet is its excellent demagnetization resistance. It can resist demagnetization forces, ensuring a stable and long-lasting magnetic performance. This makes it a reliable and durable magnet for various applications.
SmCo Magnet has exceptional magnetic properties, including a high magnetic energy product, high coercive force, and high remanence. This makes it one of the strongest permanent magnets available, with a magnetic energy product up to 30 MGOe.
SmCo Magnet is available in various shapes, including disc, cylinder, block, ring, arc, segment, etc. The most commonly used shape is the Ring SmCo Magnet, which is often used in motor and generator applications. The versatile shape options make it suitable for a wide range of applications.
Cobalt SmCo Magnet is known for its high temperature resistance, making it ideal for use in high temperature environments. It can maintain its magnetic properties even at temperatures as high as 800°C, making it suitable for use in industries such as aerospace, automotive, and energy.
SmCo Magnet is a powerful and reliable magnet that offers high performance even in harsh environments. Its unique magnetic properties and versatile shape options make it a popular choice for various industrial and technological applications.
Property | Description |
---|---|
Advantages | High Temperature Stability, High Magnetic Strength, Corrosion Resistance |
Property | Isotropic And Anisotropic Is Available |
Magnetic Properties | High Magnetic Energy Product, High Coercive Force, High Remanence |
Tolerance | 0.05mm |
Curie Temperature | 700-800°C |
Demagnetization Resistance | Excellent |
Magnetization | Multipolar Or So |
Shape | Disc, Cylinder, Block, Ring, Arc, Segment, Etc. |
Applications | Bar SmCo Magnet, Permanent Magnet SmCo, Motors, Sensors, Magnetic Couplings, Magnetic Separators, Etc. |
Mechanical Properties | Brittle, Hard, Difficult To Machine |
Grade | Residual Induction | Coercive Force | Intrinsic Coercive Force | Max. Energy Product | Max. Working Temperature | ||||||
Br | Hcb | Hcj | (BH)max | Tw | |||||||
kGs | T | kOe | KA/m | kOe | KA/m | MGOe | KJ/m³ | ℃ | |||
SmCo5 | SC16 | 8.1-8.5 | 0.81-0.85 | 7.8-8.3 | 620-660 | 15-23 | 1194-1830 | 14-16 | 110-127 | 250 | |
SC18 | 8.5-9.0 | 0.85-0.90 | 8.3-8.8 | 660-700 | 15-23 | 1194-1830 | 16-18 | 127-143 | 250 | ||
SC20 | 9.0-9.4 | 0.90-0.94 | 8.5-9.1 | 676-725 | 15-23 | 1194-1830 | 19-21 | 150-167 | 250 | ||
SC22 | 9.2-9.6 | 0.92-0.96 | 8.9-9.4 | 710-748 | 15-23 | 1194-1830 | 20-22 | 160-175 | 250 | ||
SC24 | 9.6-10.0 | 0.96- 1.00 | 9.2-9.7 | 730-770 | 15-23 | 1194-1830 | 22-24 | 175-190 | 250 | ||
Sm2Co17 | SCS22 | 9.3-9.7 | 0.93-0.97 | 8.5-9.3 | 676-740 | >18 | >1433 | 20-23 | 160-183 | 350 | |
SCS24 | 9.5-10.2 | 0.95- 1.02 | 8.7-9.6 | 692-764 | >18 | >1433 | 22-24 | 175-191 | 350 | ||
SCS24H | 9.5-10.2 | 0.95- 1.02 | 8.7-9.6 | 692-764 | >25 | >1990 | 22-24 | 175-191 | 350 | ||
SCS26M | 10.2-10.5 | 1.02- 1.05 | 8.5-9.8 | 676-780 | 12-18 | 955-1433 | 24-26 | 191-207 | 350 | ||
SCS26 | 10.2-10.5 | 1.02- 1.05 | 9.4-10.0 | 748-796 | >18 | >1433 | 24-26 | 191-207 | 350 | ||
SCS26H | 10.2-10.5 | 1.02- 1.05 | 9.4-10.0 | 748-796 | >25 | >1990 | 24-26 | 191-207 | 350 | ||
SCS28M | 10.3-10.8 | 1.03- 1.08 | 8.5-10.0 | 676-796 | 12-18 | 955-1433 | 26-28 | 207-223 | 350 | ||
SCS28 | 10.3-10.8 | 1.03- 1.08 | 9.5-10.2 | 796-812 | >18 | >1433 | 26-28 | 207-223 | 350 | ||
SCS28H | 10.3-10.8 | 1.03- 1.08 | 9.5-10.2 | 796-812 | >25 | >1990 | 26-28 | 207-223 | 350 | ||
SCS30M | 10.8-11.0 | 1.08- 1.10 | 8.5-10.5 | 676-835 | 12-18 | 955-1433 | 28-30 | 223-239 | 350 | ||
SCS30 | 10.8-11.0 | 1.08- 1.10 | 9.9-10.5 | 788-835 | >18 | >1433 | 28-30 | 223-239 | 350 | ||
SCS30H | 10.8-11.0 | 1.08- 1.10 | 9.9-10.5 | 788-835 | >25 | >1990 | 28-30 | 223-239 | 350 | ||
SCS32M | 11.0-11.3 | 1.10-1.13 | 8.5-10.7 | 676-852 | 12-18 | 955-1433 | 29-32 | 231-255 | 350 | ||
SCS32 | 11.0-11.3 | 1.10-1.13 | 10.2-10.8 | 812-860 | >18 | >1433 | 29-32 | 231-255 | 350 | ||
SCS32H | 11.0-11.3 | 1.10-1.13 | 10.2-10.8 | 812-860 | >25 | >1990 | 29-32 | 231-255 | 350 | ||
SCS35 | 11.6-12.0 | 1.16-1.20 | 10.9-11.4 | 868-908 | >18 | >1433 | 32-35 | 255-278 | 350 | ||
Low Temp Coeff Sm2Co17 | SCL18LT | 8.4-8.9 | 0.84-0.89 | 7.9-8.4 | 629-668 | >18 | >1433 | 17-19 | 135-151 | 350 | |
SCL20LT | 8.9-9.4 | 0.89-0.94 | 8.3-8.9 | 660-708 | >18 | >1433 | 19-21 | 151-167 | 350 | ||
SCL22LT | 9.4-9.8 | 0.94-0.98 | 8.7-9.3 | 692-740 | >18 | >1433 | 21-23 | 167-183 | 350 | ||
High Temp Resistance Sm2Co17 | SCG24 | 9.9-10.4 | 0.99- 1.04 | 9.3-9.9 | 740-788 | >23 | >1830 | 23-25 | 183-199 | 400 | |
SCG22 | 9.4-9.9 | 0.94-0.99 | 8.8-9.4 | 700-748 | >23 | >1830 | 21-23 | 167-183 | 450 | ||
SCG20 | 8.9-9.4 | 0.89-0.94 | 8.3-8.9 | 660-708 | >23 | >1830 | 19-21 | 151-167 | 500 |
Robust Supply Chain
Our annual production capacity is 1000 tons.
The company with China’s No.1 rare earth miner Chinalco has a
strategic partnership, with a complete production chain and a sound
quality assurance system.
Production technology leads the industry
Company covers all types of 1:5 series samarium cobalt and 2:17
series samarium cobalt full range of product numbers. It is also
one of the few domestic companies capable of producing low
temperature coeicients and the only one able to stably produce high
coercivity (Br:≥1.02T) super high temperature magnets at 550
degrees Celsius.
The coercivity of ordinary samarium cobalt magnets is approximately
2kOe. In contrast, the coercivity of our company's high-temperature
magnets remains at 6.51kOe, experiencing less than 5% loss in
magnetic properties at the same temperature.