Superalloy GH4169 Inconel 718 Rod Nickel Based Alloy Bar

Brand Name:FGD
Certification:ISO9001, ISO14000
Model Number:fgd G-012
Minimum Order Quantity:10KG
Delivery Time:3-5 days
Payment Terms:L/C, T/T, Western Union, MoneyGram
Contact Now

Add to Cart

Site Member
Location: Luoyang Henan China
Address: No. 102, Building 33, Phase II of Zhongde Industrial Park, Yibin District, Luoyang City, Henan Province
Supplier`s last login times: within 27 hours
Product Details Company Profile
Product Details
Chemical composition, %
C
Cr
Ni
Mg
Mo
Fe
≤0.08
17.0~21.0
50~55
≤0.01
2.8~3.30
Margin
Nb
B
S
Mn
Si
P
4.75~5.50
≤0.006
≤0.015
≤0.35
≤0.35
≤0.015
Cu
Ti:
Al
V
Ca
Co
≤0.30
0.65~1.15
0.30~0.7
-
≤0.01
≤1.00
Mechanical properties of GH4169 alloy at room temperature
Yield Strength
Tensile strength
Elongation
Brinell hardness
Mpa,≥
Mpa,≥
%,≥
HB
550
965
30
≤363
GH4169 Physical properties
Density
Melting point
Melting temperature range
Magnetic properties
g/cm3
8.24
1260~1340
1260~1320
Non

China Superalloy GH4169 Inconel 718 Rod Nickel Based Alloy Bar supplier

Superalloy GH4169 Inconel 718 Rod Nickel Based Alloy Bar