Add to Cart
silicon steel ei lamination transformer core silicon steel sheet price
A. The iron loss is low. A very important indicator of quality, all
countries in the world divide the grades by iron loss value. The
lower the iron loss, the higher the grade and the higher the
quality.
B. High magnetic induction intensity. Under the same magnetic
field, silicon steel sheet with high magnetic induction can be
obtained. The volume and weight of the motor or transformer core
made of it are relatively small, and relatively speaking, silicon
steel sheet, copper wire and insulating material can be saved.
C. High stacking coefficient. The surface of the silicon steel
sheet is smooth, flat and uniform in thickness, and the stacking
coefficient of the manufactured iron core is improved. Cold rolled
silicon steel sheet
D. The punching performance is good. This is more important for the
manufacture of small and micro motor cores.
E. The surface has good adhesion to the insulating film and good
solderability.
F, magnetic aging
G. The silicon steel sheet must be delivered after annealing and
pickling.
Item | Ballast Core |
Type | Steel Coil |
Thickness | 0.35 ~ 0.50mm |
Width | According to your requests |
Coil Weight | 4 ~ 8 tons |
Material | BAO Stleel: B501300, B50A1000, B50A800, B50A700, B50A600, B50A470, B35A440, B35A550, B65A600, B65A1600 B WU Steel: 50WW1300, 50WW1000, 50WW800, 50WW700, 50WW600, 50WW470, 35WW350, 35WW310, 65AW600, 65AW1600 AN Steel: 50AW1300, 50AW1000, 50AW800, 50AW700, 50AW600, 65AW1600, 65AW600, 35AW440, 35AW550 Tai Steel: 50TW290, 50TW310, 50TW470, 50TW600, 50TW800 |
Surface Treatment | C-4 Insulated Coated |
OEM and ODM | Welcome |
Application | Motor, electric engine, dynamo, transformer, electromagnetic switch, reactor, magnetic amplifiers, ballast, relay, yoke flow circle and other industry usage. |