Aerospace Industry 7075 Aluminum Round Bar / 7075 Billet Aluminum Good Stress Corrosion Control

Brand Name:HUANYU
Model Number:HYRB7075
Minimum Order Quantity:1 METRIC TON
Delivery Time:40 DAYS
Payment Terms:T/T
Place of Origin:CHINA
Contact Now

Add to Cart

Verified Supplier
Address: No. 2-4-1, Building#18, Lvcheng Street No.97, Xipeng Town, Jiulongpo District, Chongqing401326, P.R. China
Supplier`s last login times: within 2 hours
Product Details Company Profile
Product Details

7075 Aluminum Round Bar High Strength And Good Stress Corrosion Control


Aluminum Round Bar 7075


is primarily used in the aerospace industry as it is the strongest Aluminumgrade. 7075 has the strength of many steels, while retaining Aluminum’s lightweight qualities and corrosion resistance.


Application on 7075 Aluminum Round Bar


  • Highly stressed structural parts
  • Aircraft fittings
  • Gears and shafts
  • Fuse parts
  • Meter shafts and gears
  • Missile components
  • Regulating valve parts
  • Worm gears
  • Other aerospace and aircraft parts

When forging this 7075 metal, it is recommended that the temperature be set between 700 and 900 degrees F. This should then be followed by solution heat treatment. It’s not recommended for welding to be used as a joining technique, but if needed, resistance welding can be used. It’s not recommended for arc welding to be used because it can lower the metal’s corrosion resistance.


Aluminum 7075 Chemical Composition:

  • Al balance
  • Zn 5.1-6.1%
  • Mg 2.1-2.9%
  • Cu 1.2-2.0%
  • Mn 0.30%
  • Fe 0.50%
  • Si 0.40%
  • Ti 0.20%
  • Cr 0.18-0.28%


China Aerospace Industry 7075 Aluminum Round Bar / 7075 Billet Aluminum Good Stress Corrosion Control supplier

Aerospace Industry 7075 Aluminum Round Bar / 7075 Billet Aluminum Good Stress Corrosion Control

Inquiry Cart 0