Inconel 625, 2.4856, N06625, Nickel Alloy Spring Wire

Brand Name:fushun
Certification:ISO NQA
Model Number:625
Minimum Order Quantity:1KG
Delivery Time:1
Payment Terms:L/C, T/T, D/P, D/A
Contact Now

Add to Cart

Site Member
Location: Changsha Hunan China
Address: No. 812-813, Building C2, Yongsheng Commercial Plaza, 222 Labor East Road, Yuhua District, Changsha City, Hunan, China
Supplier`s last login times: within 48 hours
Product Details Company Profile
Product Details

Inconel 625, 2.4856, N06625, Nickel Alloy Spring Wire

A Nickel-Chromium-Molybdenum alloy with excellent corrosion resistance in a wide range of corrosive media, being especially resistant to pitting and crevice corrosion. Inconel 625 provides resistance to stress corrosion cracking to chloride ions, making it a favourable choice for sea water applications. The alloy also provides commendable oxidation resistance, with its high strength a result of the stiffening combination of Molybdenum and Niobium on the alloy’s Nickel-Chromium base.


Size

Diameter: 0.1 - 40mm

Shape: round, square, flat, special shaped


Key Features

Inconel 625 offers the following key features:

Excellent corrosion resistance in a wide range of corrosive media

Especially resistant to pitting and crevice corrosion

Good for sea water applications


Typical Applications

Inconel 625 is known to be suitable for the following applications:

Marine Industries

Aerospace Industries

Chemical Processing

Nuclear Reactors

Pollution Control


Designations

W.NR 2.4856

UNS N06625

AWS 012


Specifications

AMS 5666

ASTM B446

BS 3076 NA 21

ISO 15156-3

(NACE MR 0175)


Chemical Composition

ElementMin %Max %
C0.1
Mn0.5
Si0.5
P0.015
S0.015
Cr2023
Co1
Mo810
Fe5
Al0.4
Ti0.4
Ni58
Nb/Cb3.154.15
Ta0.05
Cu0.5

Physical Properties

DensityMelting PointCoefficient of ExpansionModulus of RigidityModulus of Elasticity
8.44 g/cm³1350 °C12.8 μm/m °C (20 – 100 °C)79 kN/mm²205.8 kN/mm²
0.305 lb/in³2460 °F7.1 x 10-6 in/in °F (70 – 212 °F)11458 ksi29849 ksi

Heat treatment

ConditionTypeTemperatureTimeCooling
Annealed or Spring TemperStress Relieve260 – 370°C (500 – 700°F)0.5 – 1hrAir

Mechanical Properties

Annealed
Approx. tensile strength< 1050 N/mm²< 152 ksi
Approx. operating temperature-200 to +340 °C-330 to +645 °F
Spring Temper
Approx. tensile strength1300 – 1600 N/mm²189 – 232 ksi
Approx. operating temperatureup to +200 °Cup to +395 °F