Inconel 718, 2.4668, N07718, Nickel Alloy Spring Wire

Brand Name:fushun
Certification:ISO NQA
Model Number:718
Minimum Order Quantity:1KG
Delivery Time:1
Payment Terms:L/C, T/T, D/P, D/A
Contact Now

Add to Cart

Site Member
Location: Changsha Hunan China
Address: No. 812-813, Building C2, Yongsheng Commercial Plaza, 222 Labor East Road, Yuhua District, Changsha City, Hunan, China
Supplier`s last login times: within 48 hours
Product Details Company Profile
Product Details

Inconel 718, 2.4668, N07718, Nickel Alloy Spring Wire

Nickel-Chromium alloy being precipitation hardenable and having high creep-rupture strength at high temperatures to about 700°C (1290°F). It has higher strength than Inconel X-750 and better mechanical properties at lower temperatures than Nimonic 90 and Inconel X-750. Inconel 718 has exceptional weldability compared to the Nickel-base super alloys hardened by Aluminium and Titanium.


Size

Diameter: 0.1 - 40mm

Shape: round, square, flat, special shaped


Key Features

Inconel 718 offers the following key features:

Good creep rupture strength at high temperatures

Higher strength than Inconel X-750

Better mechanical properties at lower temperatures than Nimonic 90 & Inconel X-750

Age hardenable

High temperature dynamic applications^^


Typical Applications

Inconel 718 is known to be suitable for the following applications:

Gas Turbines

Rocket Motors

Space Craft

Nuclear Reactors

Pumps

Oil & Gas Equipment


Designations

W.NR 2.4668

UNS N07718

AWS 013


Specifications

AMS 5662

AMS 5663

AMS 5832

AMS 5962

ASTM B637

GE B5OTF14/15

GE B14H89

ISO 15156-3

(NACE MR 0175)

API 6A718


Chemical Composition

ElementMin %Max %
C0.08
Mn0.35
Si0.35
P0.015
S0.015
Cr1721
Ni5055
Mo2.83.3
Nb/Cb4.755.5
Ti0.651.15
Al0.20.8
Co1
Ta0.05
B0.006
Cu0.3
Pb0.0005
Bi0.00003
Se0.0003
Febal

Physical Properties

DensityMelting PointCoefficient of ExpansionModulus of RigidityModulus of Elasticity
8.19g/cm³133 6 °C13.0 μm/m °C (20 – 100 °C)77.2 kN/mm²204.9 kN/mm²
0.296 lb/in³2437 °F7.2 x 10-6 in/in °F (70 – 212 °F)11197 ksi29719 ksi

Heat treatment

ConditionTypeTemperatureTimeCooling
No. 1 or Spring TemperAnneal980 °C (1800 °F)1hrAir
Age Harden720 °C (1330 °F)8hrFurnace
Total Age620 °C (1150 °F)18hrAir
No. 1 or Spring Temper (for ISO 15156-3 / NACE MR 0175)Anneal1010 °C (1850 °F)2hrAir
Age Harden790 °C (1455 °F)6hrAir
No. 1 Temper or Spring TemperAge Harden720 °C (1330 °F)8hrFurnace
Total Age620 °C (1150 °F)18hrAir

Mechanical Properties

Annealed
Approx. tensile strength<1000 N/mm²<145 ksi
No. 1 Temper
Approx. tensile strength1000 – 1200 N/mm²145 – 175 ksi
Spring Temper
Approx. tensile strength1250 – 1550 N/mm²180 – 225 ksi
No. 1 Temper + Annealed + Aged
Approx. tensile strength1250 – 1450 N/mm²181 – 210 ksi
Approx. operating temperature depending on load^^ and environment-200 to +550 °C-330 to +1020 °F
No. 1 Temper + Aged
Approx. tensile strength1520 – 1720 N/mm²220 – 250 ksi
Approx. operating temperature depending on load^^ and environmentContact Alloy Wire Technical Dept
Spring Temper + Annealed + Aged
Approx. tensile strength1250 – 1450 N/mm²181 – 210 ksi
Approx. operating temperature depending on load^^ and environment-200 to +550 °C-330 to +1020 °F
Spring Temper + Aged
Approx. tensile strength1700 – 1950 N/mm²247 – 283 ksi
Approx. operating temperature depending on load^^ and environmentContact Alloy Wire Technical Dept

China Inconel 718, 2.4668, N07718, Nickel Alloy Spring Wire supplier

Inconel 718, 2.4668, N07718, Nickel Alloy Spring Wire

Inquiry Cart 0